1Cr13Al4 FeCrAl Resistance Wire with 950°C Max Temperature and 1.25 ohm mm2/m Resistivity for Electric Heating
FeCrAl Allloy Strip (1Cr13Al14/CrAl14/FeCrAl134) Nominal Analysis14.00 Cr, 4.00 Al, Bal. FeMax contineous working temperature: 950º C.Melting Temperature: 1450º CElectrical Resistivity: 1.25 ohm mm2/mHas been used extensively as heating elements in industrial furnaces and electrical kilns.Has less hot strength than Tophet alloys but much higher melting point.Shanghai TANKII ALLOY MATERIAL CO., LTD.ALCHROME ALLOY PRODUCER IN CHINA Chemical Composition and Main Property of Fe